# Fusion Plating — Aluminum Anodizing Process Pack
|
||||
|
||||
Part of the Fusion Plating product family by Nexa Systems Inc.
|
||||
|
||||
Data-only module that plugs into the `fusion_plating` core and seeds the
|
||||
process taxonomy and bath chemistry schemas specific to aluminum anodizing.
|
||||
No new models, no new views — all records load with `noupdate="1"` so shop
|
||||
customisations survive module upgrades.
|
||||
|
||||
## Process types shipped
|
||||
|
||||
| Code | Name | Category |
|
||||
|---|---|---|
|
||||
| AN_TYPE_I | Type I — Chromic Acid Anodize (MIL-A-8625) | Anodizing |
|
||||
| AN_TYPE_II | Type II — Sulfuric Anodize, Clear (MIL-A-8625) | Anodizing |
|
||||
| AN_TYPE_II_DYE | Type II — Sulfuric Anodize, Dyed (MIL-A-8625) | Anodizing |
|
||||
| AN_TYPE_III | Type III — Hardcoat Anodize (MIL-A-8625) | Anodizing |
|
||||
| AN_DYE | Dye Immersion | Post-Treatment |
|
||||
| AN_SEAL_HOT | Hot Water Seal | Post-Treatment |
|
||||
| AN_SEAL_NIAC | Nickel Acetate Seal | Post-Treatment |
|
||||
| AN_SEAL_DICHRO | Dichromate Seal | Post-Treatment |
|
||||
| AN_BRIGHT | Bright Dip (Pre-Anodize) | Preparation |
|
||||
| AN_DESMUT | Desmut (Post-Etch) | Post-Treatment |
|
||||
|
||||
## Bath parameters shipped
|
||||
|
||||
Sulfuric acid concentration, dissolved aluminum, bath temperatures (Type II
|
||||
room-temp and Type III chilled), current density, voltage, chromic acid
|
||||
(Type I), seal bath temperature and pH, nickel acetate concentration, and
|
||||
dye concentration/temperature. Per-bath target overrides happen on the
|
||||
bath or recipe records in the core.
|
||||
|
||||
## Hazard awareness
|
||||
|
||||
- **Type I (chromic acid)** carries the same Cr(VI) carcinogen warnings as
|
||||
chrome plating. NPRI Part 1B reportable, Toronto Ch. 681 limits apply,
|
||||
mandatory mist suppression and medical surveillance. Prefer Type II
|
||||
wherever customer spec allows.
|
||||
- **Type II / Type III sulfuric** baths are severe splash hazards.
|
||||
Acid-resistant PPE, eyewash within 10 seconds travel, safety shower.
|
||||
- **Type III chilled bath** requires mandatory refrigeration and arc flash
|
||||
PPE at rectifier voltages up to 90 V+.
|
||||
- **Nickel acetate seal** is a WHMIS 2015 Category 1A sensitizer/carcinogen,
|
||||
subject to Ontario Reg. 833 air monitoring.
|
||||
|
||||
## Installation
|
||||
|
||||
Depends on `fusion_plating` core. Ships no security rules or views of its own.
|
||||
|
||||
```bash
|
||||
docker exec odoo-dev-app odoo -d fusion-dev -u fusion_plating_process_anodize --stop-after-init
|
||||
```
|
||||
|
||||