# Fusion Plating — Electroless Nickel Process Pack Part of the Fusion Plating product family by Nexa Systems Inc. Data-only Odoo 19 module that seeds electroless nickel (EN) plating process types and bath chemistry parameter schemas into the `fusion_plating` core. ## What ships ### Process types (`fusion.plating.process.type`) | Code | Name | Notes | |---|---|---| | `EN_LP` | Electroless Nickel — Low Phosphorus (2–5% P) | Highest hardness/wear, magnetic | | `EN_MP` | Electroless Nickel — Mid Phosphorus (6–9% P) | Workhorse EN, AMS 2404 class 4 | | `EN_HP` | Electroless Nickel — High Phosphorus (10–13% P) | Max corrosion, non-magnetic | | `EN_PTFE` | Electroless Nickel — PTFE Composite | Self-lubricating | | `EN_BNI` | Electroless Nickel — Boron Nickel | High hardness + conductivity | | `EN_STRIKE` | Nickel Strike | Pre-plate adhesion layer | ### Bath parameters (`fusion.plating.bath.parameter`) Nickel concentration, sodium hypophosphite, orthophosphite (HPO3), pH, bath temperature, metal turnovers (MTO), bath loading (dm²/L), and stabilizer. Every EN process type shares the same parameter set. Per-bath target overrides are made on the bath or recipe record in the core module. ## Hazard awareness Every process type carries `hazard_notes` flagging WHMIS 2015 Category 1A status of nickel compounds, CEPA Schedule 1 listing, hypophosphite reducer/oxidizer risks, scald PPE at 85–92 °C, Ontario Reg. 833 air monitoring, and NPRI Part 1A reporting. ## Install Requires `fusion_plating` core. No new models, views, or security rules — pure data pack loaded with `noupdate="1"` so customizations survive upgrades. ```bash docker exec odoo-dev-app odoo -d fusion-dev -u fusion_plating_process_en --stop-after-init ``` ## License OPL-1 (Odoo Proprietary License v1.0). Copyright (c) 2026 Nexa Systems Inc.